Quote:
Originally Posted by Gil View Post


Modeller,

No, I didn't think it was "kitchen aluminum foil" but "tooling foil" instead which is around 0.005" thick. You call it "tin metal from hair spray cans". Hair spray cans are made from sheet steel here in the US. If you're woking steel sheet it takes your work to a whole new level. How do you anneal the sheet during the shaping work?

-Gil
Oh)) "Taft" Hair spray You know. Then must be steel, I don't know. Without annealing Gil. Just metal shaping. Serious. Not that way the brass models are made too.