I encounter frosting using the Rust-oleum American Accents Clear. It occurs with the Matte, Gloss, and Semi Gloss. It is always an environmental issue for me. It is very hot and humid where I live. Humidity seems to be the major problem. I only have success when the humidity is between 50 and 70 percent. I have had frosting using just about any clear lacquer, regardless of the manufacturer.

Rust-oleum dries to the touch in 20 minutes and can be handled in 1 hour and is completely dry in 24 hours according to the can. To be honest, I handle it immediately and leave it in the garage overnight to dry, mainly because of the odor.

When I get frosting I let it dry completely (at least 24 hours) then re-apply when conditions are more suitable. Sometimes it works and other times I have to start all over again. That is why I scan everything.

Good luck