Mike, I've done that...in most cases you end up with a rough/raggedy side
(that isn't a huge problem)

The biggest problem is that durng the 'splitting' process, the card can buckle and bend.
And then its pretty weak after.
It never seems to hold its rigidity no matter how thick.

If its important that your card retain its rigidity and strength, you need to freshly laminate.
The glue probably adds some strength too.
Just my opinion.